Rare earth sesquioxide Lu2O3 single crystal optical fiber has a transmission wavelength range of 0.225 ~ 8 μm, its mechanical and optical properties are comparable to YAG crystals, and it has higher thermal conductivity, and its pure phase thermal conductivity can reach 12.8 W m- 1K-1, and is less affected by dopant ions, has a strong thermal management ability, and is an excellent laser gain medium. At the same time, the melting point of Lu2O3 single crystal optical fiber is 2450 °C, and its structure is stable at high temperature without phase change. It is expected to break through the upper limit of temperature measurement of traditional sapphire optical fiber, and it is a contact temperature measurement material with great potential. The company can provide Lu2O3 single crystal fiber materials grown by LHPG method, with diameters ranging from 75 to 400 μm, which can meet the needs of high-energy laser and high-temperature sensing fields.

Product parameters

Fiber orientation

<111>

Melting point

2450℃

Thermal conductivity(undoped)

~12.8 W m-1K-1

Thermal conductivity(3at.% Yb)

~10.8 W m-1K-1

Application band

from 200 nm to 8 μm

dopant ions

Yb、Nd、Ho、Er or other rare earth(Doping concentration can be customized)

diameter fluctuation

<3%

Product specification

Diameter

Maximum length

Above 400 μm email us

100~400 μm

35 cm

75~100 μm

50 cm

* 订单数量:

Number is must

* 客户姓名:

Plsease input value

* 电子邮箱:

Error E-mail format

* 手机:

Error cellphone format

* 详细地址:

Plsease input value

* 客户留言:

Plsease input value